![DurableBand-R 180μm [LL] Low Loss Large Mode Field Anti-Bending Low Water Peak Single-Mode Fiber G.652.D/G.657.A1-CDSEI](https://shopcdnpro.grainajz.com/category/348878/525/194fa28374db2f7289214494dc8bd4e7/DurableBand%20-R%20180%CE%BCm%20%5BLL%5D%20Low%20Loss%20Large%20Mode%20Field%20Anti-Bending%20Low%20Water%20Peak%20Single-Mode%20Fiber%20G.652.D-G.657.A1.webp)
- Overview
- Parameter
- Inquiry
- Related Products
DurableBand™-R 180μm [LL] G.657.A1/G.652.D low loss large mode field anti-bending low water peak single-mode fiber significantly reduces attenuation in the entire wavelength range of 1260~1625nm. Durable Band™-R 180μm [LL] exceeds the requirements of ITU-T G.652.D and ITU-T G.657.A1. It is suitable for high-capacity, long-distance transmission and access networks. This fiber optic has a cross-sectional area that is only 54% of standard fibers and 80% of 200um ordinary small diameter fibers, which helps to miniaturize equipment or accommodate more fibers under the same laying conditions. While significantly reducing the coating, it maintains the same glass outer diameter and precise geometric size control as conventional fibers, ensures low splicing loss and high splicing efficiency, excellent mechanical properties and environmental characteristics ensure stable performance of optical fibers in various usage environments.
Optical Characteristics
Attenuation
1310nm |
≤0.32 dB/km |
1383nm |
≤0.32 dB/km |
1550nm |
≤0.18 dB/km |
1625nm |
≤0.20 dB/km |
Point Discontinuity
1310/1550nm ≤0.02 dB |
Macro bending Induced Attenuation
Bending radius |
Number of Turns |
Wavelength |
Attenuation |
10mm |
1 |
1550nm |
≤0.75dB |
10mm |
1 |
1625nm |
≤1.50dB |
15mm |
10 |
1550nm |
≤0.25dB |
15mm |
10 |
1625nm |
≤1.00dB |
Cut-off Wavelength
Cable cut-off wavelength(λcc)≤1260nm |
Mode Field Diameter (MFD)
MFD at 1310nm |
9.2±0.4μm |
Dispersion
Zero-dispersion wavelength |
1300-1324nm |
Zero-dispersion slope |
0.073~0.092ps/nm2/km |
Dispersion at 1550 wavelength |
≤18.6ps/nm/km |
Polarization Mode Dispersion
Max. individual fiber PMD |
≤0.2ps/√km |
PMD link design value |
≤0.1ps/√km |
Geometric Characteristics
Cladding diameter |
125±0.7μm |
Core/clad concentricity error |
≤0.5μm |
Cladding non-circularity |
≤1.0% |
Fiber curl R |
≥4m |
Coating diameter |
180±10μm |
Coating-Cladding Concentricity |
≤10μm |
Mechanical Characteristics
Proof Test
Proof stress level |
0.90GPa(1.3%,130kpsi,11.76N) |
Strip Force
Force(peak) |
0.6N≤F≤8.9N |
Force(average) |
0.6N≤F≤5.0N |
Tensile Strength
Unaged (median; 0.5m) |
≥3.80GPa(≥550kpsi) |
Aged (median; 0.5m) |
≥3.14GPa(≥460kpsi) |
Dynamic fatigue parameters
Fatigue≥20 |
Environmental Characteristics
Test items |
Conditions |
Induced Attenuation at 1550, 1625nm |
Temperature |
-60℃ to﹢85℃ |
≤0.03dB/km |
Water Immersion |
﹢23℃/30 Days |
≤0.03dB/km |
Steady damp-heat |
﹢85℃/85%RH/30 Days |
≤0.03dB/km |
Dry heat aging |
﹢85℃/30 Days |
≤0.03dB/km |