All Categories
Inside banner

Products

DurableBand200μm Low Water Peak Single-Mode Fiber G.652.D-CDSEI

DurableBand200μm Low Water Peak Single-Mode Fiber G.652.D-CDSEI

  • Overview
  • Parameter
  • Inquiry
  • Related Products

DurableBand 200μm G.652.D low water peak single-model is applied in 1260-1625nm all band transmission systems, with low loss at 1383nm, fully utilizing E-band transmission. DurableBand 200μm exceeds the requirements of ITU-T G.652.D which is suitable for high-capacity and long-distance transmission. Smaller outer diameter size (customizable coating diameter of 180um-210um) effectively reduces the size and weight of optical cables, making it more suitable for miniaturized optical cables such as air blown micro cables. At the same time, it has the same glass outer diameter as conventional optical fibers and precise geometric dimension ensures low splicing loss and high splicing efficiency, excellent mechanical properties and environmental characteristics ensure stable performance of optical fibers in various usage environments.

 

Optical Characteristics

Attenuation

1310nm

≤0.35 dB/km

1383nm

≤0.33 dB/km

1550nm

≤0.21 dB/km

1625nm

≤0.23 dB/km

 

Point Discontinuity

1310/1550nm0.02 dB/km

 

Macro bending Induced Attenuation

Bending radius

Number of Turns

Wavelength

Attenuation

10mm

1

1550nm

≤0.75dB

10mm

1

1625nm

1.50dB

15mm

10

1550nm

≤0.25dB

15mm

10

1625nm

1.00dB

 

Cut-off Wavelength

Cable cut-off wavelength(λcc)≤1260nm

 

Mode Field Diameter (MFD)

MFD at 1310nm

8.6±0.4μm

 

Dispersion

Zero-dispersion wavelength

1300-1324nm

Zero-dispersion slope

0.092ps/nm2/km

Dispersion at 1550 wavelength

18.6ps/nm/km

 

Polarization Mode Dispersion

Max. individual fiber PMD

0.2ps/km

PMD link design value

0.1ps/km

 

Geometric Characteristics

Cladding diameter

125±0.7μm

Core/clad concentricity error

≤0.5μm

Cladding non-circularity

≤1.0%

Fiber curl R

≥4m

Coating diameter

180-210μm

Coating-Cladding Concentricity

≤10μm

 

Mechanical Characteristics

Proof Test

Proof stress level

0.90GPa(1.3%,130kpsi,11.76N)

 

Strip Force

Forcepeak)

0.6N≤F≤8.9N

Forceaverage

0.6N≤F≤5.0N

 

Tensile Strength

Unaged (median; 0.5m)

3.80GPa550kpsi)

Aged (median; 0.5m)

3.14GPa460kpsi)

 

Dynamic fatigue parameters

Fatigue≥20

 

Environmental Characteristics

Test items

Conditions

Induced Attenuation at 1550, 1625nm

Temperature

-60℃ to85℃

0.03dB/km

Water Immersion

23℃/30 Days

0.03dB/km

Steady damp-heat

85℃/85%RH/30 Days

0.03dB/km

Dry heat aging

85℃/30 Days

0.03dB/km

 